ASTM A588/A588M-2015
中文名称:最小屈服点为50 ksi (345 MPa)、抗大气腐蚀的高强度低合金结构钢规格
英文名称:Standard Specification for High-Strength Low-Alloy Structural Steel, up to 50 ksi [345 MPa] Minimum Yield Point, with Atmospheric Corrosion Resistance
原文名称:Standard Specification for High-Strength Low-Alloy Structural Steel, up to 50 ksi [345 MPa] Minimum Yield Point, with Atmospheric Corrosion Resistance
范 围:This specification covers high-strength, low-alloy structural steel shapes, plates, and bars for welded, riveted, or bolted construction with atmospheric corrosion resistance. Heat analysis shall be performed wherein the low-alloy structural steel materials shall conform to the required chemical composition for carbon, manganese, phosphorous, sulfur, silicon, nickel, chromium, molybdenum, copper, vanadium, and columbium. Steel samples shall also undergo the tensile test and conform to required values of tensile strength, yield point, and elongation.
发布日期:2015-03-01
实施日期:2015-03-01
标准组织:美国试验与材料协会标准(ASTM)
ICS分类号:(77.140.10)热处理钢
中国标准分类号:(H40)钢铁产品综合
同一中标分类下的其他标准
• AISC 303-2005建筑物和桥梁用钢铁在生产流程中的规程
• AISC ZBH 1-2000钢管的负荷和抗阻因素设计规范
• AISC ZBH 4-2000用ASTM A325或ASTM A490规定的螺栓连接钢结构件的规范
• AISC ZBH 5-2000单角钢结构构件负荷和抗阻因素设计规范
• AISC ZBH 7-1989单角钢组件安全应力设计规范
• ASTM A36/A36M-2014结构碳素钢规格
• ASTM A143/A143M-2007(R2014)
• ASTM A143/A143M-2007(2014)防止热浸镀锌结构钢制品变脆和检测变脆程序的规程
• ASTM A242/A242M-2004(2009)高强度低合金结构钢规格
版权所有:北京中科光析科学技术研究所京ICP备15067471号-33免责声明